| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Flexible C8000 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 72 | 72 | 15 sec; ASTM D2240 |
| 80 | 80 | ASTM D2240 | |
| Tensile Strength at Break | 11.7 MPa | 1700 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 5.86 MPa @Strain 100 % |
850 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 380 % | 380 % | 510 mm/min; ASTM D638 |
| Tear Strength | 43.8 kN/m | 250 pli | Die C, 510 mm/min; ASTM D624 |
| Compression Set | 23 % @Temperature 23.0 °C, Time 79200 sec |
23 % @Temperature 73.4 °F, Time 22.0 hour |
ASTM D395 |
| Clash Berg Modulus | 0.207 GPa | 30.0 ksi | ASTM D1043 |
| 0.310 GPa @Temperature -39.0 °C |
45.0 ksi @Temperature -38.2 °F |
ASTM D1043 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -37.8 °C | -36.0 °F | ASTM D746 |
| Flammability, UL94 | HB | HB | UL 94 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
| 193 - 204 °C | 379 - 399 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | NSF 51 | NATURAL, WHITE 1000, BLACK 2999. Max. Temp. of use = 100 degrees F. |
| Features | General Purpose | |
| Medium Gloss | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Coextrusion | |
| Extrusion | ||
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | General Purpose | |
| Seals | ||
| Weatherstripping |