Processing Properties Metric English Comments
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized
PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow
PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by ..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow
Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided ..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized
Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow
Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow
Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PPX-GP3 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow
Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant
Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PPX-GP8 Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 240F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Melt Temperature 274 - 302 °C
525 - 575 °F
Oxford Polymers PC/ABS 604i-FR PC/ABS, Flame retardant
Product Description: Amorphous, Polycarbonate & ABS, Flame retardant, Injection Molding Grade, VO rated @ 3.0mm. V2 rated @ 1.5mm Processing and Delivery Form: Pellets and Injection MoldingAdditive..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PPX-GP3 Modified PPO, General Purpose with HDT of 235 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy
PC/ABS Alloy, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Re..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade
PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade
PC/ABS Alloy, General Purpose, Low Gloss GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid..
Melt Temperature 274 - 327 °C
525 - 621 °F
Average value: 301 °C Grade Count:8
Overview of materials for Polycarbonate, Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr..
Melt Temperature 274 - 302 °C
525 - 575 °F
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy
General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc.
Melt Temperature 274 - 302 °C
525 - 575 °F
Star Plastics PC20NBR Molding Grade PC with Release
Information provided by Star Plastics, Inc.
Melt Temperature 274 - 302 °C
525 - 575 °F
Star Plastics PC721HFR Molding Grade PC
Information provided by Star Plastics, Inc.
Melt Temperature 274 - 302 °C
525 - 575 °F
Star Plastics PC721HFR Molding Grade PC High Flow with Release
Information provided by Star Plastics, Inc.
Melt Temperature 274 - 302 °C
525 - 575 °F
Star Plastics PC7523R Molding Grade PC
Information provided by Star Plastics, Inc.
Melt Temperature 274 - 299 °C
525 - 570 °F
Ecomass® 1700CO94 Copper Powder Filled Polyamide, Injection Molding
High Specific Gravity, Copper Powder Filled Polyamide (PA), Rigid, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInform..
Melt Temperature 274 - 302 °C
525 - 575 °F
Ecomass® 3800ZD82 Tungsten Filled Polymethylpentene
Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polymethylpentene (TPX)RigidInformation provided by Technical Polymers
Melt Temperature 274 - 316 °C
525 - 600 °F
Clariant Renol PCSP0008BK Polycarbonate, ESD Protection
Data provided by Clariant Masterbatches
Melt Temperature 274 - 316 °C
525 - 600 °F
Clariant Renol PCSP0009 Polycarbonate, 15% Glass Fiber, Silicone Lubricated
Data provided by Clariant Masterbatches
Melt Temperature 274 - 302 °C
525 - 575 °F
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.