Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-FD4 Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-UV4 Polycarbonate, UV-stabilized, Easy Flow Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
Ravago Manufacturing Americas Hylex® P1325L Polycarbonate, UV Stabilized, High Flow, Mold Release Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B.. |
|||
Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
Ravago Manufacturing Americas Hylon® N1000STHLUV2 HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat Stabilized and High FlowRoHS CompliantAuto Specifications: GM GMP.PA66.074.. |
|||
Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
MTI ThermoStran® PA66-30C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
MTI ThermoStran® PA66-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
MTI ThermoStran® PA66-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant PA131 Nylon 66, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol 6601FR Nylon 66, Flame Retardant Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol PA101F/ST801 Nylon 66, Impact Modified, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol PA101L Nylon 66, General Purpose, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol PA101LRD-190 Nylon 66, General Purpose, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant Renol PA113 Nylon 66, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant Renol PA133G33 Nylon 66, 33% Glass Fiber, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant Renol PA133GN-109 Nylon 66, High Impact, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant Renol PA1SP0005 Nylon 66, Impact Modified, Glass Reinforced Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol PA611D40 Nylon 612, Glass Fiber Reinforced, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant Renol PCSP0006 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol 6602-L Nylon 66, Internally Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol 6608-L Nylon 66, High Impact Modified, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol 6608-LLT Nylon 66, High Impact Modified, Lubricated, Low Temp Impact Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |