Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MTI ThermoStran® PA66-30C Long Carbon Fiber Compound

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Carbon Fiber Filled
Manufacturer MTI Thermoplastic Composites, Division of Montsinger Technologies, Inc. (MTI)
Trade Name ThermoStran®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MTI ThermoStran® PA66-30C Long Carbon Fiber Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent to the pellet length. Fiber / pellet length = 0.5 inches. Property values are estimated.Processing information:Mold Temperature: Higher mold temperatures are recommended for smoother surface appearance.Nozzle: Shortest length possible and 0.25 inch diameter or larger is recommended.Gates: Gates should be as large as possible and located to eliminate knit line and advantageously align fiber.Runners: Full round runners with 0.25 inch diameter and no sharp corners.Construction Material: Tool steels can be heat treated and polished to increase hardness and wear resistance. A-2 and D-2 steels can be hardened to Rockwell 60 C scale for longer life.Plating: Electroless nickel plating may offer additional wear protection.Information provided by MTI Thermoplastic Composites, Division of Montsinger Technologies, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
Filler Content 30 %
30 %
Long Carbon Fiber
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 262 MPa
38000 psi
Tensile Modulus 33.1 GPa
4800 ksi
Flexural Strength 379 MPa
55000 psi
Flexural Modulus 29.0 GPa
4200 ksi
Izod Impact, Notched 1.49 J/cm
2.80 ft-lb/in
Processing Properties Metric English Comments
Rear Barrel Temperature 260 °C
500 °F
Middle Barrel Temperature 266 °C
510 °F
Front Barrel Temperature 271 °C
520 °F
Nozzle Temperature 271 °C
520 °F
Melt Temperature 266 - 277 °C
510 - 530 °F
Mold Temperature 79.4 °C
175 °F
Drying Temperature 85.0 °C
185 °F
Dry Time 4 hour
4 hour
Dew Point -28.9 °C
-20.0 °F
Injection Pressure 68.9 MPa
10000 psi
Screw Speed 50 - 75 rpm
50 - 75 rpm
Descriptive Properties Value Comments
Nozzle ID 0.25 Inches
Screw Design 20:1 L/D