Melt Temperature |
179 - 193 °C |
354 - 379 °F |
|
PolyOne Geon™ Vinyl Rigid Extrusion 87736 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne |
Melt Temperature |
179 °C |
354 °F |
|
PolyOne Geon™ Vinyl Rigid Extrusion 87768 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Wire & Cable JA612EA Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 191 °C |
354 - 376 °F |
|
PolyOne Geon™ Vinyl Flexible A48248D Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible A5DM0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne |
Melt Temperature |
179 - 191 °C |
354 - 376 °F |
|
PolyOne Geon™ Vinyl Flexible A5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible B4D01 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible B5DW2 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 188 °C |
354 - 370 °F |
|
PolyOne Geon™ Vinyl Flexible B6000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible B8501 Polyvinyl Chloride, Flexible (PVC, Flexible)
A flexible Vinyl compound for hose and tubing applications with enhanced physical characteristics.Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible B8503 Polyvinyl Chloride, Flexible (PVC, Flexible)
A flexible PVC Compound with good resistance to migration to specific applications.Information provided by PolyOne |
Melt Temperature |
179 - 182 °C |
354 - 360 °F |
|
PolyOne Geon™ Vinyl Flexible D9501 NATURAL Polyvinyl Chloride, Flexible (PVC, Flexible)
A highly filled PVC Compound for extrusion applications.Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible F77E Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible MG23B Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible MG26 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 191 °C |
354 - 376 °F |
|
PolyOne Geon™ Vinyl Flexible R290AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible R340AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 216 °C |
354 - 421 °F |
Extrusion |
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
Melt Temperature |
179 - 188 °C |
354 - 370 °F |
|
PolyOne Geon™ Vinyl Flexible 86479 Natural Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 188 °C |
354 - 370 °F |
|
PolyOne Geon™ Vinyl Flexible 86479 Tran Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible B4DC1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible B5D01 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible B6DB1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible C5D01 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 182 °C |
354 - 360 °F |
|
PolyOne Geon™ Vinyl Flexible P484B Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible R279AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 188 °C |
354 - 370 °F |
|
PolyOne Geon™ Vinyl Flexible R336AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 182 °C |
354 - 360 °F |
|
PolyOne Geon™ Vinyl Flexible R4510H Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 185 °C |
354 - 365 °F |
|
PolyOne Geon™ Vinyl Flexible R5165A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
179 - 260 °C |
354 - 500 °F |
Average value: 229 °C Grade Count:41 |
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |