| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Rigid Extrusion 87736 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 82 | 82 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 52.2 MPa | 7570 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.78 GPa | 403 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 92.6 MPa | 13400 psi | ASTM D790 |
| Flexural Modulus | 2.99 GPa | 434 ksi | ASTM D790 |
| Izod Impact, Notched | 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
| Dart Drop Total Energy | 48.9 J/cm @Temperature 23.0 °C |
0.0916 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| 160 J/cm @Temperature 23.0 °C |
0.300 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 68.0 µm/m-°C | 37.8 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.6 °C @Thickness 3.18 mm |
150 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 179 - 193 °C | 354 - 379 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Clear/Transparent | |
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Extrusion | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Capstock | |
| Profiles |