| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 70 | 70 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 15.5 MPa | 2250 psi | Type IV, 510 mm/min; ASTM D638 |
| Tensile Strength | 7.76 MPa @Strain 100 % |
1130 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 350 % | 350 % | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -30.0 °C | -22.0 °F | ASTM D746 |
| Oxygen Index | 24 % @Thickness 3.18 mm |
24 % @Thickness 0.125 in |
ASTM D2863 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 179 - 182 °C | 354 - 360 °F | |
| 193 - 199 °C | 379 - 390 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Lubricant | |
| Appearance | Clear/Transparent | |
| Features | Good Thermal Stability | |
| High Gloss | ||
| Lubricated | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Hose | |