Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 36
36
15 sec; ASTM D2240
50
50
ASTM D2240
Tensile Strength at Break 15.9 MPa
2310 psi
510 mm/min; ASTM D638
Tensile Strength 8.27 MPa

@Strain 100 %
1200 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 350 %
350 %
510 mm/min; ASTM D638
Tear Strength 77.1 kN/m
440 pli
Die C, 510 mm/min; ASTM D624
Compression Set 60 %

@Temperature 23.0 °C,
Time 79200 sec
60 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.490 GPa
71.1 ksi
ASTM D1043
0.310 GPa

@Temperature -33.0 °C
45.0 ksi

@Temperature -27.4 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -33.3 °C
-27.9 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 179 - 185 °C
354 - 365 °F
196 - 207 °C
385 - 405 °F
Descriptive Properties Value Comments
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Hose
Tubing