| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Flexible R5165A Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 65 | 65 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 13.1 MPa | 1900 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 380 % | 380 % | Type IV, 510 mm/min; ASTM D638 |
| Tear Strength | 41.2 kN/m | 235 pli | Die C, 510 mm/min; ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -43.9 °C | -47.0 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 179 - 185 °C | 354 - 365 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Biocide | |
| Features | Good Weather Resistance | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Coextrusion | |
| Extrusion | ||
| Profile Extrusion | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Construction Applications | |
| Outdoor Applications | ||
| Profiles |