| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Flexible B5DW2 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 37 | 37 | 15 sec; ASTM D2240 |
| 50 | 50 | ASTM D2240 | |
| Tensile Strength at Break | 18.0 MPa | 2610 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 13.0 MPa @Strain 100 % |
1890 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 320 % | 320 % | 510 mm/min; ASTM D638 |
| Tear Strength | 77.8 kN/m | 444 pli | Die C, 510 mm/min; ASTM D624 |
| Compression Set | 64 % @Temperature 23.0 °C, Time 79200 sec |
64 % @Temperature 73.4 °F, Time 22.0 hour |
ASTM D395 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
| 196 - 207 °C | 385 - 405 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Medium Gloss | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Profile Extrusion | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Decorative Parts | |
| Edge Banding | ||
| Flooring | ||
| Furniture | ||
| Gaskets | ||
| Glazing | ||
| Outdoor Applications | ||
| Outdoor Furnishings | ||
| Protective Coverings | ||
| Tubing | ||
| Weatherstripping |