Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 185 - 243 °C | 365 - 469 °F | Average value: 218 °C Grade Count:8 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Melt Temperature | 221 - 243 °C | 430 - 470 °F | Molding |
PolyOne Edgetek® AS-15GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 221 - 243 °C | 430 - 470 °F | Molding |
PolyOne Edgetek® AS-30GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | Stock |
PolyOne Stat-Tech™ AS-15GF/000 SD ABS - 15% Glass Fiber Reinforced - Antistatic Protection
(discontinued **)& Data provided by PolyOne. |
|||
Melt Temperature | 232 - 243 °C | 450 - 469 °F | Extrusion |
Ineos ABS Lustran® ABS 241 ABS, Blending Grade Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 470 °F | |
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 221 - 243 °C | 430 - 470 °F | |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Melt Temperature | 232 - 243 °C | 450 - 469 °F | Injection Molding |
Ineos ABS Lustran® 261 ABS, High-Impact Blending Grade Lustran® ABS 261 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Melt Temperature | 232 - 243 °C | 450 - 470 °F | |
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black |
|||
Melt Temperature | 210 - 243 °C | 410 - 469 °F | |
Styrolution NAS® 90 High Performance Styrenic NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | |
Lubrizol Isoplast® 2530 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Melt Temperature | 210 - 243 °C | 410 - 469 °F | |
Styrolution NAS® 30 Series High Performance Styrenic It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | |
Ineos Nova Zyntar® 702 High Performance Flame Retardant Polystyrene