Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 220 - 230 °C | 428 - 446 °F | |
Polyplastic Armlen® PP MF 20-3IM Impact Modified Polypropylene Impact modified polypropylene composite materialInformation provided by PolyPlastic Group. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | |
Polimeri Europa Sinkral® B 432/E ABS Resin Sinkral B 432/E is a general purpose extrusion grade which exhibits a good balance between rigidity and toughness. Designation: Thermoplastic ISO 2580-ABS 1,EGN,105-04-16-20Applications: Large sheet.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
Polykemi AB POLYelast TPE EDS80 D35 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
NOVA Chemicals Sclair® 19G Homopolymer HDPE Film Resin Features: Excellent barrier propertiesHigh stiffnessGood processability Low gel Applications: Barrier filmsCo-extrusionDry food packagingInformation provided by Nova Chemicals |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | |
Polykemi AB POLYabs HH0 ABS, Extra Heat Resistance Information provided by Polykemi AB |
|||
Melt Temperature | 182 - 230 °C | 360 - 446 °F | Average value: 202 °C Grade Count:8 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical KEYFLEX BT 5035D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Modulus, Black ColorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical KEYFLEX BT GN7142F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Low ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP2100 PP+GF10% Description: Injection Molding, PP+GF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP2150 PP+GF15% Description: Injection Molding, PP+GF15%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene EX4 is a high density polyethylene with 1-Butene as co monomer. It is high rigidity, low gel level, high drowdown, somewhat stiffer than EX 5.Applications: film extrusion, blending partner, refuse .. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3402 PP+MF40% Description: Injection Molding, PP+MF40%, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL TE5104 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Melt Temperature | 150 - 230 °C | 302 - 446 °F | Extrusion |
Stellarchem LP-880 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Extrusion |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Flat film extrusion |
Styrolution Styrolux® 693 D SBC Description: Styrolux® 693 D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux® 693 D is mainly used for thermoformed articles, e.. |
|||
Melt Temperature | 150 - 230 °C | 302 - 446 °F | Injection Molding |
Stellarchem 475-845N TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 150 - 230 °C | 302 - 446 °F | Extrusion |
Stellarchem MP-860Q TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 210 - 230 °C | 410 - 446 °F | |
Borealis BorECO™ BA415E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO™ BA415E is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength. This material has been designed for improved processability and.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® 7010-64NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® UN-2012-L3 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Temperature | 220 - 230 °C | 428 - 446 °F | |
E-Polymers SEPAZ® LH50 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Injection molding |
BASF Ultraform® W2320 U03 POM Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion |
Polimeri Europa Koblend PD P 479 Polystyrene-Polyolefin Alloy
(discontinued **) Special polystyrene alloy for extrusion which combines very high impact strength and excellent chemical resistance to chemicals, oils and fatty foods. Koblend PD P 479 is mainly recommended as monol.. |
|||
Melt Temperature | 220 - 230 °C | 428 - 446 °F | |
Polyplastic Armlen® PP 3IM Impact Modified Polypropylene Impact modified polypropylene composite materialInformation provided by PolyPlastic Group. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
Borealis LE6006 Polyethylene It is a low loss LDPE compound for coaxial cables. LE6006 contains a special type of antioxidant, which does not adversely affect the electrical properties. Applications: bamboo constructed cables,.. |
|||
Melt Temperature | 220 - 230 °C | 428 - 446 °F | |
NOVA Chemicals Sclair® 11N1 PE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depe.. |