Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 360 - 393 °C | 680 - 739 °F | |
PolyOne Edgetek® RA-10GF-10CF/000 HI Polyphenylsulfone (PPSU) Information provided by PolyOne |
|||
Melt Temperature | 360 - 404 °C | 680 - 759 °F | Average value: 374 °C Grade Count:6 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Melt Temperature | 360 - 366 °C | 680 - 691 °F | |
LNP Lubricomp® EFL-4034 LE BK8-065 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued ** Features: Low Extractables, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Melt Temperature | 360 - 366 °C | 680 - 691 °F | |
LNP Lubricomp® EFL-4036 UFE Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Melt Temperature | 360 - 366 °C | 680 - 691 °F | |
LNP Lubricomp® EL-4030 Polyetherimide, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Melt Temperature | 360 - 366 °C | 680 - 691 °F | |
LNP Lubricomp® PDX-E-00548 CCS Polyetherimide, Aramid Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: Lubricated, Low to None Ion ContentForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however man.. |
|||
Melt Temperature | 360 - 366 °C | 680 - 691 °F | |
LNP Stat-Kon® EC-1004 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Melt Temperature | 360 - 390 °C | 680 - 734 °F | |
LATI Larpeek 50 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Melt Temperature | 360 - 391 °C | 680 - 736 °F | |
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU) Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep.. |
|||
Melt Temperature | 360 - 391 °C | 680 - 736 °F | |
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU) Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona.. |
|||
Melt Temperature | 360 - 391 °C | 680 - 736 °F | |
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU) Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha.. |
|||
Melt Temperature | 360 °C | 680 °F | Optimal |
BASF Ultrason® E 2010 MR HP PESU Description: Unreinforced, medium viscosity standard injection molding grade for improved demolding behavior with Mold Release. PES-Blend with improved processibility. (High Productivity) Abbreviate.. |
|||
Melt Temperature | 360 - 390 °C | 680 - 734 °F | |
LATI Latilub 88/50-20T PEEK, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Melt Temperature | 360 - 388 °C | 680 - 730 °F | Molding |
PolyOne Edgetek® PI-20CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 360 - 388 °C | 680 - 730 °F | Molding |
PolyOne Lubri-Tech™ PI-30GF/15T Polyetherimide (PEI), Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 360 - 390 °C | 680 - 734 °F | |
LATI Latilub 88/50-30GRT PEEK, Graphite/PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |