Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Polykemi AB POLYelast TPE HJ-75 UV Thermoplastic Elastomer, PP/Elastomer/Mineral, UV-Stabilized, Low CLTE Information provided by Polykemi AB |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
Polykemi AB POLYfill PP CIP1001F Polypropylene Information provided by Polykemi AB |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
Polykemi AB POLYfill PP CIP15015 UV Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Polykemi AB POLYfill PP CQX10030 R3 Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Melt Temperature | 230 - 270 °C | 446 - 518 °F | |
PolyOne Bergadur™ PB400 G30 H UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | Do not melt above 275°C |
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6 Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex.. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Eastman Tenite 180A-28(HT) Cellulose Acetate
(discontinued **) 28% Plasticized.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | Start Point: 250°C |
Kingfa JH830 Flame Retardant PC Features:UL V-0 @ 1.6mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInformation Prov.. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUMAX IN-5001 High Impact PBT LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
LATI Lastilac 10 ABS/PC ABS/PC Blend (ABS/PC). Unfilled. Very good surface appearance. High impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI.. |
|||
Melt Temperature | 230 - 270 °C | 446 - 518 °F | ISO 294 |
Styrolution Novodur® 4105 ABS Novodur Ultra 4105 is a PC modified high heat injection molding grade with high impact strength.Information provided by Styrolution |
|||
Melt Temperature | 230 - 270 °C | 446 - 518 °F | ISO 294 |
Styrolution Novodur® 4140PG ABS Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by .. |
|||
Melt Temperature | 230 °C | 446 °F | Injection molding |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | Injection Molding |
Styrolution Terlux® 2802 TR Q434 Transparent MABS Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Melt Temperature | 230 - 270 °C | 446 - 518 °F | Polymer Mass Temp |
Borealis Daplen™ HJ060UB Polypropylene Compound for Direct Left Manufactured Applications Daplen FJ060UB is a special low viscosity compound for direct LFT manufacturing process. It interacts perfectly with glass fibers to create excellent stiffness and impact resistance. Daplen HJ060U.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 CF10 Polyamide 6 10% Carbon Fiber - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF30 TF15 Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 MS Polyamide 6 - Natural Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For uncolored parts produced by injection molding, contain including and demo.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF20 GB10 Polyamide 6 - Glass Beads Reinforced 20% Glass fiber and 10% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following .. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV2 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, flammability class V2, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning... |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac.. |
|||
Melt Temperature | 230 - 280 °C | 446 - 536 °F | Cast-film extrusion |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF10 GB20 Polyamide 6 - Glass Beads Reinforced 10% Glass fiber and 20% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following .. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
LATI Latiblend 6252 H2 G/30 PA6/PP Homopolymer Blend based on Polyamide 6 (PA6) / Polypropylene homopolymer (PPh). Heat stabilized. Glass fibers. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |