Processing Properties | Metric | English | Comments |
---|---|---|---|
Roll Temperature | 70.0 °C | 158 °F | 3rd Roll |
Premix Thermoplastics PRE-ELEC® PC 1431 PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Roll Temperature | 70.0 °C | 158 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE.. |
|||
Roll Temperature | 70.0 °C | 158 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® CP 1315
(discontinued **) PRE-ELEC CP 1315 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Roll Temperature | 70.0 °C | 158 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® CP 1316
(discontinued **) PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resis.. |
|||
Roll Temperature | 70.0 - 100 °C | 158 - 212 °F | Top, Extrusion |
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information .. |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical LG713 ABS, Low Gloss Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Top |
LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 100 °C | 158 - 212 °F | Bottom |
LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Top |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Top |
LG Chemical LI970HF Co-Extrusion ASA Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle |
LG Chemical LI970HF Co-Extrusion ASA Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 100 °C | 158 - 212 °F | Bottom |
LG Chemical LI970HF Co-Extrusion ASA Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical MU620 ABS, Low Deformation Feature: Extrusion Molding, Low DeformationApplication: Mock-UpCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical PI641 ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 100 °C | 158 - 212 °F | Top, Extrusion |
LG Chemical PI641 ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 100 °C | 158 - 212 °F | Top, Extrusion |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 100 °C | 158 - 212 °F | Top, Extrusion |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 100 °C | 158 - 212 °F | Top, Extrusion |
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 100 °C | 158 - 212 °F | Top, Extrusion |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 100 °C | 158 - 212 °F | Top, Extrusion |
LG Chemical SH610A ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 100 °C | 158 - 212 °F | Top, Extrusion |
LG Chemical SH625 ABS, High Impact, High Flow Feature: Extrusion Molding, High Impact, High FlowApplication: Ski Flat, MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Top |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 100 °C | 158 - 212 °F | Bottom |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 100 °C | 158 - 212 °F | Top, Extrusion |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |