Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 480 - 600 min | 8.00 - 10.0 hour | Functional cure |
ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear Information provided by ITW Devcon |
|||
Cure Time | 360 - 600 min @Temperature 23.9 °C |
6.00 - 10.0 hour @Temperature 75.0 °F |
|
Master Bond EP65HT Fast Setting Epoxy Resists High Temperatures Description: Master Bond EP65HT represents a highly innovative advance in epoxy technology in that it features the unusual combination of very fast cures and high temperature resistance. While typic.. |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-15 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-15G Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-16 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-16H Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-16H-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-16RA Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-16SF-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-16S-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-17 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-18 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-18RA Dense and High-Strength Castable, Superdense Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-18SC Dense and High-Strength Castable, Superdense Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 120 - 600 min | 2.00 - 10.0 hour | Setting Time |
Chosun Refractories HSC-85AL Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 420 - 600 min | 7.00 - 10.0 hour | 1-4 hrs Air Set; 2 hrs at 200°F; 2 hrs at 500°F; 2 hrs at 700°F |
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Cure Time | 480 - 600 min | 8.00 - 10.0 hour | |
3M AC-370 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven.. |