Processing Properties Metric English Comments
Cure Time 480 - 600 min
8.00 - 10.0 hour
Functional cure
ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear
Information provided by ITW Devcon
Cure Time 360 - 600 min

@Temperature 23.9 °C
6.00 - 10.0 hour

@Temperature 75.0 °F
Master Bond EP65HT Fast Setting Epoxy Resists High Temperatures
Description: Master Bond EP65HT represents a highly innovative advance in epoxy technology in that it features the unusual combination of very fast cures and high temperature resistance. While typic..
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-15 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-15G Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-16 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-16H Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-16H-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-16RA Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-16SF-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-16S-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-17 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-18 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-18RA Dense and High-Strength Castable, Superdense
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-18SC Dense and High-Strength Castable, Superdense
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Chosun Refractories HSC-85AL Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 420 - 600 min
7.00 - 10.0 hour
1-4 hrs Air Set; 2 hrs at 200°F; 2 hrs at 500°F; 2 hrs at 700°F
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Cure Time 480 - 600 min
8.00 - 10.0 hour
3M AC-370 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven..