Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 45.0 min @Temperature 130 °C |
0.750 hour @Temperature 266 °F |
Oven |
Permabond ES550 Epoxy Resin PERMABOND ES550 is a single-part epoxy paste which is slump-resistant (does not flow) during cure. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear streng.. |
|||
Cure Time | 45.0 min @Temperature 232 °C |
0.750 hour @Temperature 450 °F |
|
Aremco Aremco-Seal™ FO-380 High Temperature Specialty Coatings Silicone, Ceramic Filled
(discontinued **) Hi-temp, waterborne silicone adhesive and sealant used to pot fiber optic strands into stainless steel ferrules. Typically used in applications to 716 °F (380 °C). Low viscosity, easy to use, offe.. |
|||
Cure Time | 45.0 min @Temperature 152 °C |
0.750 hour @Temperature 305 °F |
|
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Cure Time | 45.0 min @Temperature 152 °C |
0.750 hour @Temperature 305 °F |
|
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 8 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Cure Time | 45.0 min @Temperature 152 °C |
0.750 hour @Temperature 305 °F |
|
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 305ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Cure Time | 45.0 min @Temperature 150 °C |
0.750 hour @Temperature 302 °F |
Oven |
Permabond ES569 Epoxy Resin PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me.. |
|||
Cure Time | 45.0 - 60.0 min | 0.750 - 1.00 hour | Functional cure |
ITW Devcon 5 minute® Epoxy Gel, Opaque Information provided by ITW Devcon |
|||
Cure Time | 45.0 min | 0.750 hour | Tack-free |
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red RTV 159 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |
|||
Cure Time | 45.0 min | 0.750 hour | Tack-free |
Momentive Performance Materials RTV5243 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Cure Time | 45.0 min @Temperature 152 °C |
0.750 hour @Temperature 305 °F |
|
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Di-Cup 40C MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Cure Time | 45.0 min @Temperature 152 °C |
0.750 hour @Temperature 305 °F |
|
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 70A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Cure Time | 45.0 min @Temperature 25.0 °C |
0.750 hour @Temperature 77.0 °F |
Full Chemical |
Chesterton ARC 5ES Rapid Repair Stick Description: ARC 5ES is specifically formulated for quick reliable repairs. Its “stick” design combines the performance of a two component system with the convenience of a single component. The AR.. |
|||
Cure Time | 45.0 - 90.0 min @Temperature 22.0 °C |
0.750 - 1.50 hour @Temperature 71.6 °F |
|
Dow Corning 3-4150 DIELECTRIC GEL KIT Two-part, transparent green, fast RT or heat cure.Information provided by Dow Corning |
|||
Cure Time | 45.0 - 60.0 min | 0.750 - 1.00 hour | Tack Free Time, catalyzed with QM CAT RED 3 |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Cure Time | 45.0 min @Temperature 23.0 °C |
0.750 hour @Temperature 73.4 °F |
|
Aremco Aremco-Bond™ 820 High Performance Epoxide Clear, 1:1, 45-Minute Cure System with Good Flexibility |
|||
Cure Time | 45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
|
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Cure Time | 45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
|
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Cure Time | 45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
|
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
Cure Time | 45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
|
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
Cure Time | 45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
|
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Cure Time | 45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
|
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Cure Time | 45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
|
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Cure Time | 45.0 min @Temperature 232 °C |
0.750 hour @Temperature 450 °F |
Adequate ventilation is required when curing these products. Outgassing will occur above 300°F and cease after 750°F. An additional 30 minutes is required at the highest service temperature if service temperature is below 750°F. |
Aremco Corr-Paint™ CP4040 High Temperature Protective Coating Silicone Low viscosity, white coating for motor windings to 1100°F (593°C) |
|||
Cure Time | 45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
|
Aremco Corr-Paint™ CP4040-S1 High Temperature Protective Coating, Silicone |
|||
Cure Time | 45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
|
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||
Cure Time | 45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
|
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
Cure Time | 45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
|
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Cure Time | 45.0 - 60.0 min | 0.750 - 1.00 hour | Tack Free Time, catalyzed with QM CAT RED 3 |
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |