Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone

Category Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoset , Silicone
Manufacturer Aremco
Trade Name Corr-Paint™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
Solids Content 44.3 %
44.3 %
by Volume
57.1 %
57.1 %
by Weight
Volatile Organic Compounds (VOC) Content 587 g/l
587 g/l
Viscosity 300 - 500 cP
300 - 500 cP
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
58.4 microns
2.30 mil
estimated wet film thickness
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 593 °C
1100 °F
Continuous
Flash Point 47.8 °C
118 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 48.9 °C
50.0 - 120 °F
Application Temperature
Dry Time 1.00 - 2.00 hour
1.00 - 2.00 hour
Touch
2.00 - 4.00 hour
2.00 - 4.00 hour
Handling
1.00 - 24.0 hour
1.00 - 24.0 hour
Recoat
Cure Time >= 60.0 min
>= 1.00 hour
Air Set prior to curing
45.0 min

@Temperature 249 °C
0.750 hour

@Temperature 480 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Green
Dry Film Coverage ft2/gal 710
at 1 mil
Thinner PM Acetate