Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Di-Cup 40C

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Di-Cup 40C.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is carried out by the use of various peroxides including dicumyl peroxide (DCP) or 2,5-dimethyl-2,5-bis (t-butylperoxy) hexane (DBPH).FormulationMillathane 5004100Stearic Acid0.25N330 (HAF) Black20Di-Cup 40C3All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength, Yield 30.5 MPa
4430 psi
Elongation at Yield 570 %
570 %
300% Modulus 0.0119 GPa
1.73 ksi
Tear Strength 110 kN/m
628 pli
ASTM Die C
Processing Properties Metric English Comments
Cure Time 45.0 min

@Temperature 152 °C
0.750 hour

@Temperature 305 °F
Users viewing this material also viewed the following: