Category | Polymer , Adhesive , Thermoset , Epoxy |
Manufacturer | Aremco |
Trade Name | Aremco-Bond™ |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Aremco Aremco-Bond™ 820 High Performance Epoxide.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.15 g/cc | 1.15 g/cc | |
Viscosity | 12000 cP | 12000 cP | Mixed Viscosity |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 65 | 65 | |
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Shear Strength | 8.27 MPa | 1200 psi | ASTM D1002-94 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 28.8 µm/m-°C @Temperature 20.0 °C |
16.0 µin/in-°F @Temperature 68.0 °F |
|
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Shrinkage | 0.80 % | 0.80 % | Cure Shrinkage |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
Dielectric Constant | 6.0 @Frequency 1000 Hz |
6.0 @Frequency 1000 Hz |
|
Dielectric Strength | 33.9 kV/mm | 860 kV/in | |
Dissipation Factor | 0.040 | 0.040 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 45.0 min @Temperature 23.0 °C |
0.750 hour @Temperature 73.4 °F |
|
Pot Life | 15.0 min @Temperature 25.0 °C |
15.0 min @Temperature 77.0 °F |
100 gm mass |
Descriptive Properties | Value | Comments |
---|---|---|
Chemical Resistance | Excellent | |
Color | Clear | |
Mix Ratio By Weight | 1:1 | resin:hardener |