Aremco Aremco-Seal™ FO-380 High Temperature Specialty Coatings Silicone, Ceramic Filled  (discontinued **)

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Aremco-Seal™ FO-380 High Temperature Specialty Coatings Silicone, Ceramic Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hi-temp, waterborne silicone adhesive and sealant used to pot fiber optic strands into stainless steel ferrules. Typically used in applications to 716 °F (380 °C). Low viscosity, easy to use, offered in alternative pigments as requested.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
Solids Content 37.5 %
37.5 %
by weight
Volatile Organic Compounds (VOC) Content 60 g/l
60 g/l
Viscosity 3000 cP
3000 cP
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 380 °C
716 °F
Continuous
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Dry Time 0.5 - 1 hour
0.5 - 1 hour
Touch
1 - 2 hour
1 - 2 hour
Handling
Cure Time >= 12.0 min
>= 0.200 hour
Air Set prior to curing
45.0 min

@Temperature 232 °C
0.750 hour

@Temperature 450 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Thinner Water or MEK