Category | Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoset , Silicone |
Manufacturer | Aremco |
Trade Name | Corr-Paint™ |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.43 g/cc | 1.43 g/cc | |
Solids Content | 59 % | 59 % | by Volume |
62.1 % | 62.1 % | by Weight | |
Volatile Organic Compounds (VOC) Content | 431 g/l | 431 g/l | |
Viscosity | 150 - 250 cP | 150 - 250 cP | |
Thickness | 25.4 microns | 1.00 mil | recommended dry film thickness |
42.9 microns | 1.69 mil | estimated wet film thickness | |
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
427 °C | 800 °F | Intermittent | |
Flash Point | 46.1 °C | 115 °F |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
2.00 - 4.00 hour | 2.00 - 4.00 hour | Handling | |
1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat | |
Cure Time | >= 60.0 min | >= 1.00 hour | Air Set prior to curing |
45.0 min @Temperature 249 °C |
0.750 hour @Temperature 480 °F |
||
60.0 min @Temperature 232 °C |
1.00 hour @Temperature 450 °F |
||
Shelf Life | 6.00 Month | 6.00 Month |
Descriptive Properties | Value | Comments |
---|---|---|
Color | Blue | |
Dry Film Coverage ft2/gal | 946.7 | at 1 mil |
Primer | Not Required | |
Thinner | PM Acetate |