Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
NatureWorks® Ingeo™ 4060D Sealant Grade PLA PLA (polylactide) polymer 4060D can be coextruded with other PLA resin to form a sealant layer for biaxially oriented PLA film. This resin has excellent heat seal and hot tack performance with a sea.. |
|||
Screw Speed | 20 - 50 rpm | 20 - 50 rpm | |
MRC Polymers NAXALOYâ„¢ 793A3 GF10 PC and Polyester Blend, 10% Glass Fiber Filled 793 GF10 is available in natural and custom colors, internal and external lubricants, UV stabilizer and other modifications.Information provided by MRC Polymers Inc. |
|||
Screw Speed | 20 - 80 rpm | 20 - 80 rpm | |
Huntsman AVALON® 75 AE Thermoplastic Polyurethane Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Screw Speed | 20 - 80 rpm | 20 - 80 rpm | |
Huntsman AVALON® 80 AB Thermoplastic Polyurethane Introduction: AVALON 75 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 75 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Screw Speed | 20 - 80 rpm | 20 - 80 rpm | |
Huntsman AVALON® 90 AKU Thermoplastic Polyurethane Introduction: AVALON 90 AKU is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same ha.. |
|||
Screw Speed | 20 - 50 rpm | 20 - 50 rpm | |
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU), 20% Glass Fiber Veradel® 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Screw Speed | 20 - 50 rpm | 20 - 50 rpm | |
Lubrizol Estane® 58144 Thermoplastic Polyurethane Type: Estane® 58144 is a 65D Polyether-type thermoplastic polyurethane (TPU) compound.Features: FDA (contact Lubrizol for details). Pre-drying: 2 hours at 104C (220F) in Dehumidifying Hopper Dryer.. |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant 6004G8-HSL BK UV Black Nylon 6, 8% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant PA213N40 Nylon 6, Mineral/Glass Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol 60G13HSP Black Nylon 6, 13% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol 60G33-L Nylon 6, 33% Glass Fiber Reinforced, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA113G15 Nylon 66, 15% Glass Fiber Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA113G33HR Nylon 66, 33% Glass Fiber, Heat Stabilized, Hydrolysis Resistant Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA123G13 Nylon 66, 13% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA211G40 Nylon 6, 40% Glass Fiber, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA211N40 Nylon 6, Mineral/Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA223G13 Nylon 6, 13% Glass Fiber, Impact Modified Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PBT1700 Polybutylene Terephthalate, Flame Retardant Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PCSP0006WT-181 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PP1100G40 Polypropylene Homopolymer, 40% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PPSP0004 Polypropylene, Random Copolymer Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol TPU1088A Polyurethane Elastomer, Aromatic Polyester Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol 6602-L Nylon 66, Internally Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol 6608G43 Nylon 66, 43% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol 6608-LLT Nylon 66, High Impact Modified, Lubricated, Low Temp Impact Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol BR7039G15 Nylon 6, 15% Glass Fiber, bondable to TPU Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 100 rpm | 20 - 100 rpm | |
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Screw Speed | 20 - 50 rpm | 20 - 50 rpm | |
Clariant Renol PPSS0007 Polyphenylene Sulfide, Glass Fiber and Mineral Filled Data provided by Clariant Masterbatches |