Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NatureWorks® Ingeo™ 4060D Sealant Grade PLA

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polylactic Acid (PLA) Biopolymer
Manufacturer NatureWorks LLC
Trade Name Ingeo™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NatureWorks® Ingeo™ 4060D Sealant Grade PLA.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PLA (polylactide) polymer 4060D can be coextruded with other PLA resin to form a sealant layer for biaxially oriented PLA film. This resin has excellent heat seal and hot tack performance with a seal initiation temperature of 80ºC. This sealant does not adversely affect the unique properties of NatureWorks® PLA bioriented film such as high gloss and transparency, dead-fold or aroma and grease barrier.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D1505
Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 80.0 °C
176 °F
ASTM F88
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 52.0 - 58.0 °C
126 - 136 °F
ASTM D3417
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ASTM D1003
Gloss 90 %
90 %
20°; ASTM D1003
Processing Properties Metric English Comments
Feed Temperature 180 °C
356 °F
Adapter Temperature 200 °C
392 °F
Die Temperature 190 °C
374 °F
Melt Temperature 210 °C
410 °F
Drying Temperature 45.0 °C

@Time 14400 sec
113 °F

@Time 4.00 hour
Moisture Content <= 0.025 %
<= 0.025 %
Dew Point -35.0 °C
-31.0 °F
Drying Air Flow Rate >= 14.2 l/min
>= 0.500 ft³/min (CFM)
Screw Speed 20 - 100 rpm
20 - 100 rpm