Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL EC-605B Electrically Conductive POM, 5% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL HI-515 High Impact POM, Unreinforced LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL MR-310 Low Warpage POM, 10% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL N115 POM, Unreinforced, High Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL VC127-LD Antistatic POM, Unreinforced, High Flow, For VCR Reels LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | Injection Molding |
LG Chemical LUCON 6080EX ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUCON SP9306FL sPS+MF Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 .. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUMAX HR-5306F Heat Resistant PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL GP-1000FA General Purpose Polypropylene, High Impact, Flame Retardant, Non-Bleed LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUPOS GP-2201F General Purpose ABS, 20% Glass Fiber Reinforced, Flame Retardant LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY EC5000A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Anti-Static.Application: E&E (Housing)Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1000L PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY HI1002ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY HP5004A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SR3108L PC, High Impact Description: Injection Molding, PC, High Flow, High Impact, White Color OnlyApplication: BLU Mold frame for Mobile DevicesCAS: 103598-77-2 and 13463-67-1Information provided by LG Chemical |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL GP-3154F General Purpose Polypropylene, 15% Mineral Fillers, High Modulus, Flame Retardant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL TE-5005H Thermoplastic Elastomer Alloy, Dimensional Stability LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL TE-5102 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUPOS GP-2200H General Purpose ABS, 20% Glass Fiber Reinforced, High Heat Resistance LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical Lupox® GP-1001F General Purpose PBT, Unreinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical Lupox® SG-4405 Surface Gloss PBT, 40% Glass Fiber/Mineral Reinforced, Dimensional Stability LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow Description: Injection Molding, PC, Halogen Free Flame Retardant, High Flow, High ImpactApplication: IT/OA (M/P Battery Inner Pack Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information pro.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1000MD PC, Light Diffusion Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1006FM PC, Flame Retardant Description: Injection Molding, PC, Flame RetardantApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |