Processing Properties Metric English Comments
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant 6008 L Nylon 6, High Impact, Injection Molding
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant ABS4500G30 ABS, 30% Glass Reinforced
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant PA123G30 Nylon 66, 30% Glass Fiber, Impact Modified, Heat Stabilized
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol 6001 HV HSL Nylon 6, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol 60G33-L Nylon 6, 33% Glass Fiber Reinforced, Lubricated
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol ABS3460 ABS, General Purpose, Low Gloss
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol ABS5475 ABS, General Purpose, Low Gloss
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol BR7008 Polycarbonate/Polyester Alloy
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol BR7140 Polycarbonate/ABS Alloy
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PA111G50IF Nylon 66, 50% Glass Fiber, Improved Flow
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PA113G33HR Nylon 66, 33% Glass Fiber, Heat Stabilized, Hydrolysis Resistant
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PA2SP0004 Nylon 6 Alloy
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PA2SP0008HW Nylon 6, Heavyweight Compound
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PA2SP0017 Nylon 6, Impact Modified
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PA2SP0023 Nylon 6, Impact and Flow Modified, ESD Protection
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PBT1100TF10 Polybutylene Terephthalate, PTFE Lubricated
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PC010-L FR Polycarbonate, Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PCSP0006WT-181 Polycarbonate, Laser Markable
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PP1112AS10 Polypropylene, Static Dissipative
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PPA1100G50 Polyphthalamide, 50% Glass Fiber
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PPOSP0001 Polyphenylene Oxide, Mineral Filled
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PPSP0006HW Polypropylene Homopolymer, Heavy Weight Compound
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Remafin PESP0006 High Density Polyethylene, 10% Glass Fiber
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol 6601M Nylon 66, Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol 6608-L UV Black Nylon 66, High Impact Modified, Lubricated, UV Stable
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol 6622-L Nylon 66, Glass Fiber Filled, Lubricated
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Clariant Renol PPSP0005 Polypropylene Homopolymer, Glass Fiber and Mica Reinforced, Chemically Coupled