Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Capron® 8331G HI HS BK-102 Impact Modified, 14% Glass-Filled Nylon 6 (Dry)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Filled, Impact Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Capron® 8331G HI HS BK-102 Impact Modified, 14% Glass-Filled Nylon 6 (Dry)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Capron 8331G HI HS BK-102 is a black pigmented, heat stabilized, 30% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of strength, stiffness and excellent moldability/surface aesthetics. It is also available in non-heat stabilized (Capron 8331G HI).Capron 8331G HI HS BK-102 is generally recommended for applications such as front wheel chair wheels, bicycle wheels, power tool housings, chain saw housings, clips and fasteners, hose clamps and window hardware.Data provided by Allied Signal.Processing: Max. water content 0.12%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.Melt Temperature: 270-295 degC (518-563 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics critical, a mold surface temperature of 80-95 degC (176-203 degF) is required. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate. Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO data
Water Absorption 1.2 %
1.2 %
24 hrs; ISO data
Moisture Absorption at Equilibrium 1.8 %
1.8 %
50% RH; 23°C; ISO data
Water Absorption at Saturation 7.0 %
7.0 %
in water; 23°C; ISO data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 90.0 MPa
13100 psi
ASTM data at 5 mm/min.
92.0 MPa
13300 psi
ISO value at 5mm/min.
Flexural Yield Strength 150 MPa
21800 psi
ASTM Data
Flexural Modulus 4.14 GPa
600 ksi
ASTM Data
Poissons Ratio 0.35
0.35
ISO data
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM and ISO test
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Processing Properties Metric English Comments
Drying Temperature 85.0 °C
185 °F
See Materials Notes