Polymer Property : Drying Temperature = 200 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 82.2 - 93.3 °C
180 - 200 °F
Polymer Resources ABS-FR Flame Retardant ABS
Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch..
Drying Temperature 82.2 - 93.3 °C
180 - 200 °F
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and..
Drying Temperature 82.2 - 93.3 °C
180 - 200 °F
Polymer Resources ABS-GP1 General Purpose ABS
General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Drying Temperature 82.2 - 93.3 °C
180 - 200 °F
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized
General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In..
Drying Temperature 87.8 - 93.3 °C
190 - 200 °F
PTS Trilac® ABS-HH2500 Super High Heat ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Drying Temperature 87.8 - 93.3 °C
190 - 200 °F
PTS Trilac® ABS-HS4000 General Purpose ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Drying Temperature 87.8 - 93.3 °C
190 - 200 °F
PTS Trilac® ABS-HS5500 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Drying Temperature 87.8 - 93.3 °C
190 - 200 °F
PTS Trilac® ABS-HS7500 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Drying Temperature 87.8 - 93.3 °C
190 - 200 °F
PTS Trilac® ABS-MP1000 Metal Plating Grade ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Drying Temperature 82.2 - 93.3 °C
180 - 200 °F
PolyOne Lubri-Tech™ PS-30GF/15T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated  (discontinued
Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Drying Temperature 87.8 - 93.3 °C
190 - 200 °F
PTS Trilac® ABS-HF5500 High Flow ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Drying Temperature 60.0 - 93.3 °C
140 - 200 °F
Average value: 81.0 °C Grade Count:9
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a..
Drying Temperature 82.2 - 93.3 °C
180 - 200 °F
During prolong interruptions the hopper dryer temperature should be reduced to 65ºC or lower.
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
Drying Temperature 82.2 - 93.3 °C
180 - 200 °F
Star Plastics ABS405 Extrusion Grade ABS
Information provided by Star Plastics, Inc.
Drying Temperature 82.2 - 93.3 °C
180 - 200 °F
Star Plastics ABSLG5035 Molding Grade ABS, Low Gloss
Information provided by Star Plastics, Inc.
Drying Temperature 76.7 - 93.3 °C
170 - 200 °F
4 to 24 hrs; Tray Dryer
Shuman 730 Utility White ABS
Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the Shuman Plastics, Inc.
Drying Temperature 87.8 - 93.3 °C
190 - 200 °F
TPI Porene® ABS-GA800 High Impact ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Drying Temperature 87.8 - 93.3 °C
190 - 200 °F
TPI Porene® ABS-KU650 Super High Heat ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Drying Temperature 65.6 - 93.3 °C
150 - 200 °F
Desiccant type
CPT C-Flex® R70-003 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Drying Temperature 65.6 - 93.3 °C
150 - 200 °F
Desiccant type
CPT C-Flex® R70-026 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Drying Temperature 65.6 - 93.3 °C
150 - 200 °F
Desiccant type
CPT C-Flex® R70-028 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Drying Temperature 65.6 - 93.3 °C
150 - 200 °F
Desiccant type
CPT C-Flex® R70-046 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Drying Temperature 65.6 - 93.3 °C
150 - 200 °F
Desiccant type
CPT C-Flex® R70-072 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Drying Temperature 87.8 - 93.3 °C
190 - 200 °F
Chi Mei Polylac® PA-747 ABS
High impact
Drying Temperature 65.6 - 93.3 °C
150 - 200 °F
Desiccant type
CPT C-Flex® R70-085 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Drying Temperature 65.6 - 93.3 °C
150 - 200 °F
Desiccant type
CPT C-Flex® R70-214 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Drying Temperature 87.8 - 93.3 °C
190 - 200 °F
Chi Mei Polylac® PA-765 ABS - Flame Retardant
F.R. High Flow
Drying Temperature 65.6 - 93.3 °C
150 - 200 °F
Desiccant type
CPT C-Flex® R70-251 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Drying Temperature 82.2 - 93.3 °C
180 - 200 °F
LTL Color Compounds ColorFast® GPA300 ABS
Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc.
Drying Temperature 82.2 - 93.3 °C
180 - 200 °F
LTL Color Compounds ColorFast® GPA300X ABS
Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc.