Processing Properties Metric English Comments
Drying Temperature 75.0 - 107 °C
167 - 225 °F
Average value: 85.1 °C Grade Count:16
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Drying Temperature 75.0 - 80.0 °C
167 - 176 °F
LG Chemical LI-921 ASA, Extrusion, High Stiffness
Information Provided by LG Chem
Drying Temperature 75.0 - 85.0 °C
167 - 185 °F
LG Chemical HF-350 ABS, High Flow, High Impact
Information Provided by LG Chem
Drying Temperature 75.0 - 85.0 °C
167 - 185 °F
Injection Molding
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Drying Temperature 75.0 - 80.0 °C

@Time 14400 sec
167 - 176 °F

@Time 4.00 hour
Chi Mei Acryrex® CM-207 PMMA
Features:General PurposeGood Weather ResistanceHigh GlossHigh Heat ResistanceHigh StrengthMedium ViscosityUses: Automotive Interior PartsBathroom AccessoriesContainersCosmeticsHousehold GoodsKnobsRo..
Drying Temperature 75.0 - 85.0 °C
167 - 185 °F
Eurostar Staramide AG6H PA66, 30% Glass Filled, Injection Molded
AG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Staramide AS10 PA66, 50% Glass Bead Reinforced, Injection Molding
Staramide AS10 is a 50% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding
Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C
167 - 185 °F
Eurostar Staramide BG10H PA6, 50% Glass Filled, Injection Molded
BG10 is a Heat Stabilized, 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Drying Temperature 75.0 - 85.0 °C
167 - 185 °F
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded
BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Staramide BK8 PA6, 40% Mineral Fiber Filled, Injection Molded
Staramide BK8 is a 40% Mineral Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C
167 - 185 °F
Eurostar Staramide BST42 PA6, Impact Modified, Injection Molded
BST42 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Staramide P1000IX2 PA6, Impact Modified, Injection Molded
Staramide P1000IX2 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI010 or Star X 2010)Information provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Staramide PF005 PA6, 25% Glass Fiber Filled, Injection Molded
Staramide PF005 is an 25% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Staramide PF006ES PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF006ES is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Staramide PX08000 PA6, Impact Modified, Injection Molded
Staramide PX08000 is an Impact Modified Polyamide 6 Injection Molding Resin (also known as Star X 2006)Information provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Staramide RF004XXC PA6, 20% Glass Fiber Filled, Injection Molded
Staramide RF004XXC is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Staramide RF00AES PA66/6, 50% Glass Filled, Injection Molded
Staramide RF00AES is a 50% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 50V S3)Information provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Staramide RF00ASXP PA66, 50% Glass Filled, Injection Molded
Staramide RF00ASXP is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 G 50V S3)Information provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C
167 - 185 °F
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded
AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Starflam P10002Z PA6, Flame Retardant, Extrusion
Starflam P10002Z is an Unfilled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Extrusion ResinInformation provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Starflam RF0059 PA66, Glass Fiber, Flame Retardant, Injection Molded
Starflam RF0059 is a Flame Retardant, Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Eurostar Staramide PF003U PA6, 15% Glass Fiber Filled, Injection Molded
Staramide PF003U is an 15% Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin, UV Stabilized (also known as Staramide 6 15V S4)Information provided by Eurostar.
Drying Temperature 75.0 - 100 °C

@Time 7200 - 14400 sec
167 - 212 °F

@Time 2.00 - 4.00 hour
Azoty Tarnow™ Tarnamid® T-27 CF20 Polyamide 6 20% Carbon Fiber- Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Drying Temperature 75.0 - 100 °C

@Time 7200 - 14400 sec
167 - 212 °F

@Time 2.00 - 4.00 hour
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced
30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Drying Temperature 75.0 - 100 °C

@Time 7200 - 14400 sec
167 - 212 °F

@Time 2.00 - 4.00 hour
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T..
Drying Temperature 75.0 - 100 °C

@Time 7200 - 14400 sec
167 - 212 °F

@Time 2.00 - 4.00 hour
Azoty Tarnow™ Tarnamid® T-27 GF10 MX6 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T..
Drying Temperature 75.0 - 100 °C

@Time 7200 - 14400 sec
167 - 212 °F

@Time 2.00 - 4.00 hour
Azoty Tarnow™ Tarnamid® T-29 Polyamide 6 - Natural
Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.Tarn..
Drying Temperature 75.0 - 100 °C

@Time 7200 - 14400 sec
167 - 212 °F

@Time 2.00 - 4.00 hour
Azoty Tarnow™ Tarnamid® T-27 GF35 Polyamide 6 - Glass Fiber Reinforced
35% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..