Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i.. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-GP2-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Rear Barrel Temperature | 243 - 293 °C | 470 - 560 °F | |
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Rear Barrel Temperature | 243 - 293 °C | 470 - 560 °F | |
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan.. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Rear Barrel Temperature | 260 - 293 °C | 500 - 560 °F | |
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled 13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 260 - 293 °C | 500 - 560 °F | |
LTL Color Compounds ColorFast® NY2GF131 Nylon 66, 13% Glass-Filled, Impact Modified 13% glass-filled impact modified nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
LTL Color Compounds ColorFast® PC100 Polycarbonate 10 melt standard injection molding gradeAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
Wellman EcoLon® MRGF1616-BK 40% Mineral/Glass Reinforced Post Consumer Compound Nylon 6 Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 6Information provided by Wellman. |
|||
Rear Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Rear Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
Wellman Wellamid® 22LHI6 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Rear Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
Wellman Wellamid® 22LH-N Unfilled Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Rear Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
Wellman Wellamid® 22L-N Unfilled Nylon 66, Lubricated Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Rear Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Rear Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Rear Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Rear Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Rear Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
Wellman Wellamid® XT1486-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Rear Barrel Temperature | 243 - 293 °C | 470 - 560 °F | |
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
LTL Color Compounds ColorFast® FRPC400 Polycarbonate, Flame-Retarded Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 260 - 293 °C | 500 - 560 °F | |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |