Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA)
(Unverified Data**) Ixef 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance. - Natural: Ixef.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA)
(Unverified Data**) Ixef 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss. - B.. |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Compression Zone |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 2057 Polyarylamide (PARA), 45% Mineral Filler
(discontinued **) Ixef 2057 is a 45% mineral-reinforced polyarylamide which exhibits high strength and stiffness, and outstanding surface gloss. Due to its mineral reinforcement, Ixef 2057 resin mold with very low wa.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler
(discontinued **) Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe.. |
|||
Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID GP2330A(W) PA6+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Cooling Fan), E&E (Bobbin)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5000GU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Info.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5000HU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 26062-94-2, 137050-02-03 and 103598-77-2Information provided by LG Chemical |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5000S PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5000SP PBT+PC Description: Injection Molding, PBT+PC, Low Gloss, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5006F PET+PC Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5011M PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG .. |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUPOY RF3208F PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2 and 13463-67-1Information provided by LG .. |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUPOY SR3108L PC, High Impact Description: Injection Molding, PC, High Flow, High Impact, White Color OnlyApplication: BLU Mold frame for Mobile DevicesCAS: 103598-77-2 and 13463-67-1Information provided by LG Chemical |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Start Point: 255°C |
Kingfa PC-WT01 Weather Resistance PC Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec.. |
|||
Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance.Features: Go.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without s.. |
|||
Rear Barrel Temperature | 250 °C | 482 °F | |
Solvay Specialty Polymers Omnix® FC-9050 Polyamide, High Performance (HPPA), 50% Glass Fiber Omnix® FC-9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Rear Barrel Temperature | 250 °C | 482 °F | |
Tipco Tipcofil® AG 800 - 40% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 40% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 1 |
Eurostar Staramide AST43 PA66, Impact Modified, Injection Molded AST43 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Elastocon TPE Technologies Elastocon® STK56PA Thermoplastic Elastomer Elastocon® STK56PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA is well suited for consumer go.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Compression Zone |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, at Equilibrium (65% RH)
  Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Compression Zone |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical |