Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
Multibase Multi-Pro® 0612 CW Polypropylene Calcium carbonate filler, 6% filer by weightForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
Multibase Multi-Pro® 2518 CU Polypropylene Calcium Carbonate Filler, 25% by weight.Features:Gloss, High Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
Multibase Multi-Pro® 3019 CXUW Polypropylene Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov.. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT1055-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT2600-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Interior trimSplash shieldsStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT3080-425 Thermoplastic Polyolefin, UV Stabilized, YBWA Platinum Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products HP513-01 High Stiffness Polypropylene Copolymer, Medium Impact, UV Stabilized, Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P102-00 Polypropylene, Black Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P107-00 Polypropylene Homopolymer, Natural Applications: Wire harnessesTrim componentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P251-00 Polypropylene Copolymer, Natural Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products P252-00 Polypropylene Copolymer, Natural Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
Oxford Polymers ABS 20CCF-MP-BK ABS, 20% Carbon Fiber Reinforced Conductive Carbon Fiber (20% Reinforced), ABS injection molding grade Processing and Delivery Form: Pellets and extrusion/Injection Molding Additives: Release AgentsInformation provided by Oxford P.. |
|||
Rear Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
Polymer Resources ABS-GP1 General Purpose ABS General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Rear Barrel Temperature | 188 °C | 370 °F | |
ExxonMobil Vyram™ 9101-45 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Rear Barrel Temperature | 188 °C | 370 °F | |
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Rear Barrel Temperature | 188 °C | 370 °F | |
ExxonMobil Vyram™ 9101-75 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Rear Barrel Temperature | 188 °C | 370 °F | |
ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
RheTech Products HP513-00A High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 188 - 218 °C | 370 - 425 °F | |
Star Plastics ABS405 Extrusion Grade ABS Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 188 - 218 °C | 370 - 425 °F | |
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 188 - 218 °C | 370 - 425 °F | |
Star Plastics ABS3545 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,.. |
|||
Rear Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc.. |
|||
Rear Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
LTL Color Compounds ColorFast® GPA300X ABS Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc. |