Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers TEKALOY® S630XB Heat Resistance, Weatherability PC/PBT Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKALOY®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKALOY® S630XB Heat Resistance, Weatherability PC/PBT Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability. PC/PBT is usually used for automotive applications with good resistance against oils and solvents as well as high impact. PC/PET has an excellent surface and its high heat resistance allows it to be employed in housing for electrical appliances.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength 68.67 MPa
9960 psi
ASTM D638
Elongation at Break 90 %
90 %
ASTM D638
Flexural Strength 88.29 MPa
12810 psi
ASTM D790
Flexural Modulus 2.403 GPa
348.6 ksi
ASTM D790
Izod Impact, Notched 1.96 J/cm
3.67 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 260 - 280 °C
500 - 536 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F