Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 155 - 180 °C | 311 - 356 °F | |
Resinoid 2225 Phenolic Molding, Cellulose Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-8032/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-8086/YL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-8087/BL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15/BK PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-7836 PPS, linear, with glass fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts.High dim.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8095 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.High chemic.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8400 PPS, linear, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8457 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-8217 Polyether imide, with PTFE, lubricant modified Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Control disks, cams, slidi.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-7575 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
LATI Latiohm 88/10-06 CNT PEEK Semiconductive/dissipative product based on Polyetheretherketone (PEEK). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK) AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. .. |
|||
Mold Temperature | 140 - 180 °C | 284 - 356 °F | |
Eurotec® Tecomid® NT40 CR30 BK111 HS PPA, 30% carbon fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 140 - 180 °C | 284 - 356 °F | |
Eurotec® Tecomid® NT40 NL XA60 PPA, unfilled, flame retardant - halogen & red phosphorus free, heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The .. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-7742 Polyether imide, with glass fiber, demolding aid Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8291 PPS, linear, with aramid reinforcement Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma.. |