Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer Amity Thermosets
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowApplications: Electric motor commutators ( medium mechanical strength )Motor starter partsSignaling equipment partsHigh voltage electric meter coversCircuit protecting switchesElectric relay parts which ought to withstand high voltage Automotive parts ( spacers, spark plugs etc )Components which ought to withstand electric shock but not high mechanical stressComponents which ought to be dimensionally stable electrically insulating & resistant to humidity, etc. Information provided by Amity Thermosets Limited
Physical Properties Metric English Comments
Density 1.68 - 1.78 g/cc
0.0607 - 0.0643 lb/in³
Molding; IS 867-1963
Apparent Bulk Density 0.700 - 0.850 g/cc
0.0253 - 0.0307 lb/in³
IS 867-1963
Water Absorption 0.12 - 0.25 %
0.12 - 0.25 %
IS 13411-1993
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
IS 13411-1992
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 - 45.0 MPa
4350 - 6530 psi
5 mm/min.; IS 867-1963
Shear Strength 50.0 - 65.0 MPa
7250 - 9430 psi
IS 867-1963
Izod Impact, Notched 0.150 - 0.250 J/cm
0.281 - 0.468 ft-lb/in
IS 13411-1992
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 - 1.00e+13 ohm-cm
1.00e+12 - 1.00e+13 ohm-cm
IS 3396-1979
Surface Resistance 3.2e+11 - 1.0e+12 ohm
3.2e+11 - 1.0e+12 ohm
IS 3396-1979
Dielectric Strength 8.00 - 10.5 kV/mm

@Temperature 90.0 °C
203 - 267 kV/in

@Temperature 194 °F
IS 2584-1963
Processing Properties Metric English Comments
Mold Temperature 160 - 180 °C
320 - 356 °F
Injection Pressure 14.7 - 35.28 MPa
2130 - 5117 psi
Mold Pressure
Cure Time 0.917 - 1.08 min
0.0153 - 0.0181 hour
per mm
Shelf Life 12.0 Month
12.0 Month
10-25°C
Descriptive Properties Value Comments
Chloride content Nil to traces
Free Phenol Nil to traces