Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Average value: 80.4 °C Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® S600F10 BK851 PBT
(Unverified Data**) Crastin® S600F10 BK851 is an unreinforced, lubricated, medium high viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® S600F40 BK851 PBT
(Unverified Data**) Crastin® S600F40 BK851 is an unreinforced, lubricated, low viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® S620F20 BK851 PBT
(Unverified Data**) Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® SK602 BK851 PBT
(Unverified Data**) Crastin® SK602 BK851 is a 15% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® SK605 BK851 PBT
(Unverified Data**) Crastin® SK605 BK851 is a 30% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Injection Molding |
DuPont Performance Polymers Crastin® SK615SF BK591 PBT
(Unverified Data**) Crastin® SK615SF BK591 is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast .. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Injection Molding |
DuPont Performance Polymers Crastin® SK615SF NC010 PBT
(Unverified Data**) Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® SK642FR BK851 PBT
(Unverified Data**) Crastin® SK642FR BK851 is a black 15% glass fiber reinforced, flame retardant polybutylene terephthalate for injection molding. It has a UL94 V-0 rating @ 0.75mm.Information provided by DuPont Perf.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® ST820 BK503 PBT
(Unverified Data**) Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | Start Point: 90°C |
Kingfa JH710 G10D Flame Retardant & 10% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:Exact mechanism partsElectrical and elect.. |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | Start Point: 90°C |
Kingfa JH720 G10D 10% Glass Fiber Reinforced PC Features:Good processing propertiesLow tendency to warpHigh mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanne.. |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | Start Point: 90°C |
Kingfa JH720 G20 20% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
Lanxess Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral PET + PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Mold Temperature | 110 - 130 °C | 230 - 266 °F | |
LATI Lasulf PSU Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
LATI Latishield 85-08A G/20 PES, Steel/Glass Fibers EMI shielding product based on Polyether Sulfone (PES). Steel fibers. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
Solvay Specialty Polymers Kalix® 3850 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 3850 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in.. |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
Solvay Specialty Polymers Kalix® 3950 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 3950 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in.. |
|||
Mold Temperature | 110 - 130 °C | 230 - 266 °F | actual surface temp |
Unitika PT-3020 Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd. |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
Covestro Makrolon® 1095 Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min15 % Glass fiber reinforcedHigh viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CExtrusionAvailable .. |
|||
Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFLR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityUV stab.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® S600LF NC010 PBT Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Mold Temperature | 120 - 130 °C | 248 - 266 °F | |
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Mold Temperature | 85.0 - 130 °C | 185 - 266 °F | DAM |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® CE2055 BK580 PBT
(Unverified Data**) Crastin® CE2055 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® HR5330HF BK503 PBT
(Unverified Data**) Crastin® HR5330HF is a 30% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® LW9030 BK851 PBT
(Unverified Data**) Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Injection Molding |
DuPont Performance Polymers Crastin® S610SF NC010 PBT
(Unverified Data**) Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Informati.. |