| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Average value: 74.3 °C Grade Count:32 |
| Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Average value: 80.4 °C Grade Count:14 |
| Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
| DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**) Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
| DuPont Performance Polymers Crastin® LW9320 BK851 PBT
(Unverified Data**) Crastin® LW9320 BK851 is a 20% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
| DuPont Performance Polymers Crastin® LW9320LM BK591 PBT
(Unverified Data**) Crastin® LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It has excellent surface aspect, dimensional stability and low warpage and was developed fo.. |
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
| DuPont Performance Polymers Crastin® S600F40 BK851 PBT
(Unverified Data**) Crastin® S600F40 BK851 is an unreinforced, lubricated, low viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
| DuPont Performance Polymers Crastin® S620F20 BK851 PBT
(Unverified Data**) Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly.. |
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Injection Molding |
| DuPont Performance Polymers Crastin® SK612SF NC010 PBT
(Unverified Data**) Crastin® SK612SF is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Injection Molding |
| DuPont Performance Polymers Crastin® SK615SF BK591 PBT
(Unverified Data**) Crastin® SK615SF BK591 is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast .. |
|||
| Mold Temperature | 120 - 130 °C | 248 - 266 °F | |
| LATI LASULF Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | Start Point: 90°C |
| Kingfa JH710 G15 Flame Retardant & 15% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | Start Point: 90°C |
| Kingfa JH720 G20 20% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | Injection Molding |
| LG Chemical LUCON SP9306FL sPS+MF Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 .. |
|||
| Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
| Lanxess Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral PET + PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | Start Point: 100°C |
| Kingfa JH710 G30 Flame Retardant & 30% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
| Solvay Specialty Polymers Kalix® 3850 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 3850 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in.. |
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
| Solvay Specialty Polymers Kalix® 3950 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 3950 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in.. |
|||
| Mold Temperature | 115 - 130 °C | 239 - 266 °F | |
| Solvay Specialty Polymers Kalix® 5950 HFFR Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impa.. |
|||
| Mold Temperature | 110 - 130 °C | 230 - 266 °F | |
| Covestro Apec® 1703 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=171 °CPreprocessingMax. Water content |
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
| Covestro Makrolon® 1095 Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min15 % Glass fiber reinforcedHigh viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CExtrusionAvailable .. |
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
| Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel.. |
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
| Covestro Makrolon® GF8001* Polycarbonate, 20% Glass Filled ISO 7391-PC,MR,(,,)-18-3,GF20Developmental productFormerly Makrolon DP1-1951MVR (300 °C/1.2 kg) 16 cm3/10 min20 % Glass fiber reinforcedLow viscosityEasy releaseInjection molding - Melt temperature.. |
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
| DuPont Performance Polymers Crastin® CE2056 NC010 PBT Crastin® CE2056 NC010 is an unreinforced polybutylene terephthalate molding resin.Information provided by DuPont Performance Polymers |
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
| DuPont Performance Polymers Crastin® S600LF NC010 PBT Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
| Covestro Makrolon® DP1-1888* Polycarbonate, 20% Glass Filled ISO 7391-PC,MR,(,,)-09-3,GF20Developmental productMVR (300 °C/1.2 kg) 10 cm3/10 min20 % Glass fiber reinforcedMilled fiberMedium viscosityEasy releasegood surface qualityInjection molding - Melt te.. |
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
| Covestro Makrolon® GF8002* Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Formerly Makrolon DP1-1882MVR (300 °C/1.2 kg) 9.5 cm3/10 min15 % Glass fiber reinforcedMedium viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CAva.. |
|||
| Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
| Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
| Mold Temperature | 120 - 130 °C | 248 - 266 °F | |
| LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
| Mold Temperature | 120 - 130 °C | 248 - 266 °F | |
| LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Injection Molding |
| DuPont Performance Polymers Crastin® S610SF NC010 PBT
(Unverified Data**) Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Informati.. |
|||