Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Mold Temperature = 240 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-BR1 Polycarbonate, Branched for Extrusion and Blow Molding
Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical and thermal te..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigm..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced
Polycarbonate, 10% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-G10-IM Polycarbonate, 10% Glass Reinforced, Impact Modified
Polycarbonate, 10% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-G20-[color]-WS Polycarbonate, 20% Glass Reinforced
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced
Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-G40-[color]-1 Polycarbonate, 40% Glass Reinforced with Mold Release
Polycarbonate, 40% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow
Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release
Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-GP2-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Medium Flow
Polycarbonate, 5% PTFE, General Purpose, Medium Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release
Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-GP1-TFE10 Polycarbonate, 10% PTFE, Wear Resistant, Low Flow
Polycarbonate, 10% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant
Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Mold Temperature 65.6 - 116 °C
150 - 240 °F
Average value: 85.7 °C Grade Count:8
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
Mold Temperature 82.2 - 116 °C
180 - 240 °F
LTL Color Compounds ColorFast® PCGF110 Polycarbonate, 10% Glass-Filled
High modulus 10% glass-filled polycarbonate, V2-rated, general purposeAll information provided by LTL Color Compounders, Inc.
Mold Temperature 82.2 - 116 °C
180 - 240 °F
LTL Color Compounds ColorFast® PCGF130 Polycarbonate, 30% Glass-Filled
30% glass-filled grade polycarbonateAll information provided by LTL Color Compounders, Inc.
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Copyright © lookpolymers.com All Rights Reserved