Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 100 °C | 212 °F | Injection Molding |
Covestro Apec® DP 1-9339/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Mold Temperature | 100 °C | 212 °F | DAM; optimum |
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66
(Unverified Data**) Minlon® 11C140 BK086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 100 °C | 212 °F | DAM; optimum |
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**) Zytel® FE270038 is a 40% glass fiber/mineral reinforced, heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.Information provided by DuPont Performan.. |
|||
Mold Temperature | 100 °C | 212 °F | DAM; optimum |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK261 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 for injection molding. It has excellent surface appearance and gloss.Information provided by Du.. |
|||
Mold Temperature | 100 °C | 212 °F | DAM; optimum |
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6
(Unverified Data**) Zytel® 73G45 BK263 is a 45% glass fiber reinforced, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 100 - 150 °C | 212 - 302 °F | |
Lehmann & Voss LUVOCOM® 1501/CF/30-1 Polysulfone, with carbon fiber Applications: Automotive industry, office machinery, medical- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Chemical and hydrolysis resistance parts, non.. |
|||
Mold Temperature | 100 - 120 °C | 212 - 248 °F | |
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Mold Temperature | 100 - 120 °C | 212 - 248 °F | |
LATI Latilon 28D PC Polycarbonate (PC). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability. Very good surface appearanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Mold Temperature | 100 °C | 212 °F | |
Taiwan PU Corporation PTMG CPU-100L Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Mold Temperature | 100 - 110 °C | 212 - 230 °F | actual surface temp |
Unitika TERRAMAC TE-7000 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Mold Temperature | 100 - 110 °C | 212 - 230 °F | actual surface temp |
Unitika TERRAMAC TE-7300 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Mold Temperature | 100 - 110 °C | 212 - 230 °F | actual surface temp |
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Mold Temperature | 100 °C | 212 °F | Injection Molding; ISO 10724 |
Covestro Apec® 1745 Polycarbonate Easy to demoldsuitable for superheated steam sterilization up to 143 °C as well as for pharmaceutical applications according to United States Pharmacopeia (USP) XXII Class VIsoftening temperature (.. |
|||
Mold Temperature | 100 °C | 212 °F | Injection Molding; ISO 10724 |
Covestro Apec® 1795 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content |
|||
Mold Temperature | 100 °C | 212 °F | Injection Molding; ISO 10724 |
Covestro Apec® 1800 Polycarbonate Basic gradesoftening temperature (VST/B 120)=185 °CPreprocessingMax. Water content |
|||
Mold Temperature | 100 °C | 212 °F | Injection Molding; ISO 10724 |
Covestro Apec® 2095 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=203 °CPreprocessingMax. Water content |
|||
Mold Temperature | 100 °C | 212 °F | Optimal |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Mold Temperature | 100 °C | 212 °F | Optimal |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Mold Temperature | 100 °C | 212 °F | Optimal |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Mold Temperature | 100 °C | 212 °F | Optimal |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |
|||
Mold Temperature | 100 - 150 °C | 212 - 302 °F | |
LATI LAESTRA G/40-V0CT1 40% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Mold Temperature | 100 °C | 212 °F | optimum |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Mold Temperature | 100 °C | 212 °F | optimum |
DuPont Performance Polymers Sorona® 3301V NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3301V NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for applications requiring high surface gloss in a broad.. |
|||
Mold Temperature | 100 °C | 212 °F | DAM; optimum |
DuPont Performance Polymers Zytel® 73G30TGI BK267 Nylon 6
(Unverified Data**) Zytel® 73G30TGI BK267 is a 30% glass fiber reinforced, toughened, black polyamide 6 optimized for gas injection molding process.Information provided by DuPont Performance Polymers |