Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
SABIC M40053S High Density Polyethylene for Injection Molding Product Description: M40053S is a UV stabilized high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to pro.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
SABIC PP 49MK40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 49MK40 is a high crystalline impact copolymer with high stiffness. This grade is especially developed for producing injection molded articles. The grade contains an antist.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
SABIC PP 513MN40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 513MN40 is a controlled rheology PP grade of narrow molecular weight distribution. It contains an antistatic agent and is especially developed for producing injection molde.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
SABIC PP 5702P Polypropylene Homopolymer for Injection Molding Product Description: PP 5702P is specially developed for rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the products.Typical.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
SABIC PP 5703P Polypropylene Homopolymer for Injection Molding Product Description: PP 5702P is specially developed for producing rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the produc.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
SABIC PP 578P Polypropylene Homopolymer for Injection Molding Product Description: PP 578P is a controlled rheology PP grade of medium molecular weight distribution suitable for injection molding applications. It gives consistent processability, good flow pr.. |
|||
Mold Temperature | 15.0 - 15.0 °C | 59.0 - 59.0 °F | (close to) |
Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding The Trithene® SX 7010 resin is a medium molecular weight, low-density polyethylene (LDPE) which allows the production of flasks with an adequate combination of mechanical and impact strength, flexi.. |
|||
Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
SABIC M200024 Linear Low Density Polyethylene for Injection Molding Product Description: M200024 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to give good f.. |
|||
Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
SABIC M300054 High Density Polyethylene for Injection Molding Product Description: M300054 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow.. |
|||
Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
SABIC M80064 Series High Density Polyethylene for Injection Molding Product Description: M80064 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good rigid.. |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet.. |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
Inno-Comp INNOPOL® CS 3-8000 FR Flame Retardant Polypropylene Blend INNOPOL® CS 3-8000 FR is a flame retarded polypropylene compound based on a specific blend of polypropylene homo polymer and copolymer. This grade is available in natural and custom colored form... |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
Inno-Comp INNOPOL® CS 1-2120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL CS 1-2120 AP is a 20 % talc filled compound based on polypropylene homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 1-2120 AP is recommended especially.. |
|||
Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
Borealis HH315MO Polypropylene HH315MO is a polypropylene homopolymer intended for injection molding. Its high melt flow makes it especially suitable for products with long flow length. This grade is designed for high-speed injec.. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
Borealis RJ370MO Polypropylene, Transparent Random Copolymer RJ370MO is a specially modified highly-transparent polypropylene random copolymer with very high melt flow rate. It is designed for high-speed injection molding and contains nucleating and demoldin.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS1110UVI Polymer, Natural Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS1900HF Polymer, Natural Durastar DS1900HF polymer is a high flow grade of Durastar . Durastar DS1900HF flow lengths are increased 20-40% relative to Durastar DS1000 as shown by spiral flow testing. Other outstanding featur.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS1910HF Polymer, Natural Durastar DS1910HF polymer is a high flow grade of Durastar that contains a mold release. Durastar DS1910HF flow lengths are increased 20-40% relative to Durastar DS1010 as shown by spiral flow testi.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS2000 Polymer, Natural Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has ver.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS2110UVI Polymer, Natural Durastar DS2110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar MN620 Polymer, Natural Applications:Blood therapyDrug deliveryIV componentsMedicalSurgical instrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAProduct Description: DuraStar Poly.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar MN621 Polymer, Natural Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman Eastar AN014 Copolyester Eastar AN014 copolyester is a high flow product that contains a mold release. Eastar AN014 flow lengths are increased 20-40% relative to Eastar AN004 as shown by spiral flow testing. Other outstandi.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman Eastar DN001HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN001HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | EBM |
Eastman Tritan TX1801 Copolyester, Natural Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo.. |
|||
Mold Temperature | 15.0 - 95.0 °C | 59.0 - 203 °F | |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
LATI Latimass 37 B01-01 D025 Bio-Polymer Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
Borealis Borsoft™ SG220MO Polypropylene Random Copolymer for Injection Molding Borsoft™ SG220MO is a polypropylene characterized by good flow, high impact and good transparency. This grade contains antistatic and demolding additives which, together with enhanced nucleation, .. |