Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 225 - 280 °C | 437 - 536 °F | Average value: 246 °C Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | Average value: 263 °C Grade Count:12 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Nozzle Temperature | 235 - 280 °C | 455 - 536 °F | Average value: 263 °C Grade Count:3 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 3-7088-1 Polyamide 6, with carbon fiber and glass fiber, low-warpage Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 3-7234-1 Polyamide 6, with carbon fiber, electrically conducting Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressAntistatic.Handles, levers, rollers, body parts.Information provided by L.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 3-7451 Polyamide 6, lubricant modified, heat stabilized Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 3-7901 Polyamide 6, with glass fiber and carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 3-8266/BL Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 3-8363 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID GN-2251BF Flame Retardant PA Alloy Feature: Injection Molding, Flame Retardant PA AlloyApplication: E&E partsInformation provided by LG Chemical |
|||
Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUMID GP2130AE PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Industrial MaterialCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical |
|||
Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUMID HI1102A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: H/Lamp Screw MountingCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | |
LG Chemical Lupox® PBT-HI1002FM Impact Modified, Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided.. |
|||
Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUPOY HP5004A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
LG Chemical LUPOY HR-5006A Heat Resistant PC/ABS Alloy, Unreinforced, Weather Resistant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
LG Chemical LUPOY HR-5007AX Heat Resistant PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
Nozzle Temperature | 275 - 280 °C | 527 - 536 °F | |
Lavergne VYTEEN PC/ABS 8515XF Polycarbonate - Acrylonitrile Butadiene Styrene Alloy Vyteen PC/ABS 8515XF is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High d.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | |
Gromax CCP PET 9130-200 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |