Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6 Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au.. |
|||
Nozzle Temperature | 255 - 270 °C | 491 - 518 °F | |
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical Lupox® TE5000HU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 26062-94-2, 137050-02-03 and 103598-77-2Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical Lupox® TE5000HZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Door Handle)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical Lupox® TE5000LZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provide.. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical Lupox® TE5006F PET+PC Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Nozzle Temperature | 235 - 270 °C | 455 - 518 °F | Injection Molding |
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio.. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax PBT 4130-104D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax PBT 4130-201D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Lavergne VYPET VNT 1021 Polyester-PC Alloy The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical Lupox® TE5011 PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Samyang Tribit® 1500G30 Polybutylene Terephthalate, 30% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Unitika AX-1500 Conditioned AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Unitika AXF-1500-05 Conditioned Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Unitika AXG-1500-300 Conditioned Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Tisan TISLAMID® 66 20% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Tisan TISLAMID® 66 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Unitika UM-8400-20 Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Nozzle Temperature | 250 - 270 °C | 482 - 518 °F | |
Unitika UM-8430RG Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Nozzle Temperature | 200 - 270 °C | 392 - 518 °F | |
Arkema Group Pebax® MX 1205 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MX 1205 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arke.. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax PBT 4115-201D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 265 - 270 °C | 509 - 518 °F | |
Beijing Chemical Industry KAIFA® MN201-G10 Nylon 66 Resin 10% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 265 - 270 °C | 509 - 518 °F | |
Beijing Chemical Industry KAIFA® MN201-G35 Nylon 66 Resin 35% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 265 - 270 °C | 509 - 518 °F | |
Beijing Chemical Industry KAIFA® MN301-G25 Nylon 66 Resin 25% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 265 - 270 °C | 509 - 518 °F | |
Beijing Chemical Industry KAIFA® MN301-G30 Nylon 66 Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |