| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT) |
| Manufacturer | LG Chemical |
| Trade Name | Lupox® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LG Chemical Lupox® TE5011 PBT+PC.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.020 | 0.020 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm <br>@Thickness 3.20 mm |
0.0070 - 0.010 in/in <br>@Thickness 0.126 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 47.1 MPa <br>@Thickness 3.20 mm |
6830 psi <br>@Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Break | >= 100 % <br>@Thickness 3.20 mm |
>= 100 % <br>@Thickness 0.126 in |
50mm/min; ASTM D638 |
| Flexural Yield Strength | 68.6 MPa <br>@Thickness 6.40 mm |
9960 psi <br>@Thickness 0.252 in |
2.5mm/min; ASTM D790 |
| Flexural Modulus | 1.86 GPa <br>@Thickness 6.40 mm |
270 ksi <br>@Thickness 0.252 in |
2.5mm/min; ASTM D790 |
| Izod Impact, Notched | 1.47 J/cm <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C |
2.76 ft-lb/in <br>@Thickness 0.126 in,<br> Temperature -22.0 °F |
ASTM D256 |
| NB <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C |
NB <br>@Thickness 0.126 in,<br> Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 225 °C | 437 °F | @ Break; ASTM D3418 |
| Deflection Temperature at 0.46 MPa (66 psi) | 110 °C <br>@Thickness 6.40 mm |
230 °F <br>@Thickness 0.252 in |
Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C <br>@Thickness 6.40 mm |
194 °F <br>@Thickness 0.252 in |
Unannealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
| Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
| Front Barrel Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
| Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
| Melt Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Injection Molding |
| Drying Temperature | 120 °C | 248 °F | Injection Molding |
| Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |