Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | |
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 243 - 260 °C | 469 - 500 °F | |
LNP VALOX® SMV5847 PBT + PET Alloy, 30% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. VC3000.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data .. |
|||
Nozzle Temperature | 250 - 260 °C | 482 - 500 °F | Average value: 255 °C Grade Count:4 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Nozzle Temperature | 250 - 260 °C | 482 - 500 °F | |
Lehmann & Voss LUVOCOM® 6-7834 Polyamide 12, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion, for dimensional stable precision parts.Isotropic sh.. |
|||
Nozzle Temperature | 250 - 260 °C | 482 - 500 °F | |
Lehmann & Voss LUVOCOM® 6-8395 Polyamide 12, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s.. |
|||
Nozzle Temperature | 250 - 260 °C | 482 - 500 °F | |
Lehmann & Voss LUVOCOM® 6-8436 Polyamide 12, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve.. |
|||
Nozzle Temperature | 250 - 260 °C | 482 - 500 °F | |
Lehmann & Voss LUVOCOM® 6-8503/BL Polyamide 12, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve.. |
|||
Nozzle Temperature | 250 - 260 °C | 482 - 500 °F | |
Lehmann & Voss LUVOCOM® 6-8548 Polyamide 12, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab.. |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | |
Firestone CLM200-001 Nylon 6 Used for monofiliament extrusion. Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | |
Firestone CR212-203-D Nylon 6, Heat Stabilized Black color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3 mm.Information provided by Firestone |
|||
Nozzle Temperature | 240 - 260 °C | 464 - 500 °F | |
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® SV1120M PBT Description: Injection Molding, PBT, General Purpose, High ViscosityApplication: Films & Sheets, Optical Loose TubeCAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 246 - 260 °C | 475 - 500 °F | Injection Molding |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |
|||
Nozzle Temperature | 245 - 260 °C | 473 - 500 °F | Injection Molding |
Ineos ABS Lustran® ABS 248FC Medical & Food Contact Grade Lustran® ABS 248FC resin is a high-gloss, medium-impact grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of physical properties and has been desi.. |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Nozzle Temperature | 250 - 260 °C | 482 - 500 °F | |
Gromax PBT 2000-104D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Nozzle Temperature | 250 - 260 °C | 482 - 500 °F | |
Gromax PBT 2000-201D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Nozzle Temperature | 241 - 260 °C | 465 - 500 °F | |
Solvay Technyl® C216V25 25% Glass Filled Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Nozzle Temperature | 243 - 260 °C | 470 - 500 °F | |
Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled Plate-able. Natural and colors available. Injection molding grade. Uses: Automotive, appliancesInformation provided by Engineered Polymer Solutions. |
|||
Nozzle Temperature | 246 - 260 °C | 475 - 500 °F | |
Calsak CS-72 General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Nozzle Temperature | 246 - 260 °C | 475 - 500 °F | |
Calsak CS-72L General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Nozzle Temperature | 240 - 260 °C | 464 - 500 °F | |
BLUESTAR PBT 6630 30% Glass Filled PBT6630 is an injection molding grade, with 30% glass fiber reinforced, high heat stability, and electrical properties, easy to process. It is widely used in automotive, home appliance, E/E industry.. |