Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Nozzle Temperature = 200 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 200 °C
392 °F
Premix Thermoplastics PRESEAL® TPE 5020
General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o..
Nozzle Temperature 200 - 220 °C
392 - 428 °F
Noltex Soarnol® D2908 Ethylene Vinyl Alcohol Copolymer
Ethylene content 29 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..
Nozzle Temperature 200 - 274 °C
392 - 525 °F
Average value: 230 °C Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Nozzle Temperature 200 - 210 °C
392 - 410 °F
Huntsman AVALON® 98 AB Thermoplastic Polyurethane
Introduction: AVALON 98 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 98 AB is part of the AVALON Performance Range and offers a premium soling ma..
Nozzle Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical HI100 ABS, High Impact
Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
Nozzle Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical HT700 ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Nozzle Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
LG Chemical KEYFLEX BT 1040D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Nozzle Temperature 200 - 220 °C
392 - 428 °F
LG Chemical LUCEL EC-605B Electrically Conductive POM, 5% Carbon Black Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Nozzle Temperature 200 - 220 °C
392 - 428 °F
LG Chemical LUCEL GB-325 Low Warpage POM, 25% Glass Bead Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Nozzle Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity
Feature: Injection Molding, POM+GF40%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
Nozzle Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical SG175 ABS, Super Surface Gloss
Feature: Injection Molding, Super Surface GlossApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
Nozzle Temperature 200 - 220 °C
392 - 428 °F
Lehmann & Voss LUVOCOM® TPE-7711/GY Thermoplastic elastomer, with carbon fiber, electrically conducting
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Bearings, sleeves, sliding elements, chair rollers, handles.Info..
Nozzle Temperature 200 - 220 °C
392 - 428 °F
Lehmann & Voss LUVOCOM® TPE-7829 Thermoplastic elastomer, with PTFE
Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K..
Nozzle Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
LG Chemical XG569C MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical
Nozzle Temperature 200 °C
392 °F
Lubrizol Advanced Materials PEARLTHANE® D11H92S Thermoplastic Polyurethane Elastomer
PEARLTHANE® D11H92S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out..
Nozzle Temperature 200 - 215 °C
392 - 419 °F
Lubrizol Estane® S195A Thermoplastic Polyurethane
Type: Estane® S195A is a Shore 95A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
Nozzle Temperature 200 °C
392 °F
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Nozzle Temperature 200 °C
392 °F
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Nozzle Temperature 200 °C
392 °F
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Nozzle Temperature 200 °C
392 °F
Tisan TISOPLEN® 40% Talc Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Nozzle Temperature 200 °C
392 °F
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Nozzle Temperature 200 °C
392 °F
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized, Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Nozzle Temperature 200 - 210 °C
392 - 410 °F
Injection
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
Nozzle Temperature 200 - 235 °C
392 - 455 °F
Elastocon TPE Technologies Elastocon® SMR1450 Thermoplastic Polyolefin Elastomer
Elastocon® SMR1450 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E..
Nozzle Temperature 200 - 205 °C
392 - 401 °F
Injection
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer
Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 200 - 205 °C
392 - 401 °F
Injection
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer
Zythane™ 6075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 200 - 215 °C
392 - 419 °F
Injection
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer
Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 200 - 240 °C
392 - 464 °F
Injection Molding
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Nozzle Temperature 200 - 240 °C
392 - 464 °F
Injection Molding
LG Chemical KEYFLEX TO1088AV Olefin Type TPE
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0Information provided by LG Chemical
Copyright © lookpolymers.com All Rights Reserved