| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 199 - 235 °C | 390 - 455 °F | |
| ExxonMobil Santoprene® 241-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
| Nozzle Temperature | 215 - 235 °C | 419 - 455 °F | Injection Molding |
| LG Chemical KEYFLEX BT 1245D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Medium Modulus, Black colorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
| Nozzle Temperature | 220 - 235 °C | 428 - 455 °F | |
| Lubrizol Estane® S368D Thermoplastic Polyurethane Type: Estane® S368D is a Shore 68D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
| Nozzle Temperature | 225 - 235 °C | 437 - 455 °F | Injection |
| Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
| Nozzle Temperature | 191 - 235 °C | 375 - 455 °F | |
| ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
| Nozzle Temperature | 199 - 235 °C | 390 - 455 °F | |
| ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
| Nozzle Temperature | 199 - 235 °C | 390 - 455 °F | |
| ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
| Nozzle Temperature | 199 - 235 °C | 390 - 455 °F | |
| ExxonMobil Santoprene® 271-87 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
| Nozzle Temperature | 200 - 235 °C | 392 - 455 °F | |
| Elastocon TPE Technologies Elastocon® SMR1000 Thermoplastic Polyolefin Elastomer Elastocon® SMR1000 thermoplastic polyolefin elastomer has been developed for applications that require impact resistance and a high gloss scratch and mar resistant surface finish. Elastocon® SMR10.. |
|||
| Nozzle Temperature | 200 - 235 °C | 392 - 455 °F | |
| Elastocon TPE Technologies Elastocon® SMR1450 Thermoplastic Polyolefin Elastomer Elastocon® SMR1450 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E.. |
|||
| Nozzle Temperature | 200 - 235 °C | 392 - 455 °F | |
| Elastocon TPE Technologies Elastocon® SMR1555 Thermoplastic Polyolefin Elastomer Elastocon® SMR1555 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E.. |
|||
| Nozzle Temperature | 200 - 235 °C | 392 - 455 °F | |
| Elastocon TPE Technologies Elastocon® SMR1600 Thermoplastic Polyolefin Elastomer Elastocon® SMR1600 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E.. |
|||
| Nozzle Temperature | 225 - 235 °C | 437 - 455 °F | |
| Lubrizol Estane® S375D Thermoplastic Polyurethane Type: Estane® S375D is a Shore 78D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
| Nozzle Temperature | 199 - 235 °C | 390 - 455 °F | |
| ExxonMobil Santoprene® 221-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
| Nozzle Temperature | 199 - 235 °C | 390 - 455 °F | |
| ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||