Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Oxford Polymers PC 714-FR Series PC, Flame retardant Product Description: Amorphous, Polycarbonate injection molding grade, flame retardant Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and UV stabilizersSpecial.. |
|||
Front Barrel Temperature | 288 - 299 °C | 550 - 570 °F | |
Polymer Resources NY6/12-G43 Nylon 612, 43% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Polymer Resources NY66-G20-MD Nylon 66, 20% Glass Reinforced with MoS2 Nylon 66, 20% Glass Reinforced with Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigment.. |
|||
Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Polymer Resources NY66-G60 Nylon 66, 60% Glass Reinforced Nylon 66, 60% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Polymer Resources NY6-G50 Nylon 6, 50% Glass Reinforced Nylon 6, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Front Barrel Temperature | 271 - 299 °C | 520 - 570 °F | |
Polymer Resources PPX/NY GP1 PPO/Nylon 66 Alloy Polyphenylene Oxide/Nylon 66 Alloy , General PurposeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylex® P1010LLT Polycarbonate Information provided by Ravago. |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylex® P1310LLT Polycarbonate Information provided by Ravago |
|||
Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PTS Tristar® PC-10 10 MFI Extrusion Grade Polycarbonate Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PTS Tristar® PC-10R-(IM) 10 MFI Impact Modified Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Polymer Resources NY66-G55 Nylon 66, 55% Glass Reinforced Nylon 66, 55% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PTS Tristar® PC-10R 10 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PTS Tristar® PC-10R-(V) 10 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PTS Tristar® PC-10R-CL 10 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 299 °C | 520 - 570 °F | |
Wellman Wellamid® GFT15N050-N2 15% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
&n Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Mitsubishi Iupilon® S2000UR 9.5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Mitsubishi Iupilon® S2001R 9.5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 299 °C | 520 - 570 °F | |
Wellman Wellamid® GF33-66 XE-N, 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Front Barrel Temperature | 271 - 299 °C | 520 - 570 °F | |
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Front Barrel Temperature | 271 - 299 °C | 520 - 570 °F | |
Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Front Barrel Temperature | 271 - 299 °C | 520 - 570 °F | |
Wellman Wellamid® GF43-66/6 XE-N 43% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Front Barrel Temperature | 271 - 299 °C | 520 - 570 °F | |
Wellman Wellamid® GF60-66/6 XE-N 60% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Front Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Entec Hylex® P1310FR Polycarbonate Information provided by Ravago |
|||
Front Barrel Temperature | 271 - 299 °C | 520 - 570 °F | |
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |