Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 221 - 260 °C | 430 - 500 °F | |
Multibase Multi-Pro® 4005 M Polypropylene Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Front Barrel Temperature | 221 - 260 °C | 430 - 500 °F | |
Multibase Multi-Pro® 4010 M Polypropylene Mica Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses:Pump PartsInformation provided by Multibase |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products CC40P100-00 40% Calcium Carbonate Reinforced Polypropylene, Natural Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products CC40P100-00EG 40% Calcium Carbonate Reinforced Polypropylene, Natural, Extrusion Grade Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products F56-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 221 - 260 °C | 430 - 500 °F | |
Multibase Multi-Pro® 4005 MI Polypropylene Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Front Barrel Temperature | 221 - 243 °C | 430 - 470 °F | |
LTL Color Compounds ColorFast® ACR100IM Polymethylmethacrylate, High Impact High impact version, extrusion or injection molding PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 221 - 254 °C | 430 - 490 °F | |
LTL Color Compounds ColorFast® PBA2000 PBT/ABS Alloy, Flame Retarded Flame-retarded V0-rated PBT/ABS alloyAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Multibase Multi-Flex® D 5308 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
Front Barrel Temperature | 221 - 232 °C | 430 - 450 °F | |
Multibase Multi-Flex® 1047-2000 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
Front Barrel Temperature | 221 - 238 °C | 430 - 460 °F | |
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black |
|||
Front Barrel Temperature | 221 - 227 °C | 430 - 440 °F | |
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Front Barrel Temperature | 221 - 227 °C | 430 - 440 °F | |
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;.. |
|||
Front Barrel Temperature | 221 - 227 °C | 430 - 440 °F | |
Teknor Apex Telcar® TL-8451 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Front Barrel Temperature | 221 - 227 °C | 430 - 440 °F | |
Teknor Apex Telcar® TL-8730 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Front Barrel Temperature | 221 °C | 430 °F | |
Lubrizol ESTALOC® 59104 Ester-Type, Reinforced Engineering Thermoplastic Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impactUses: Injection Molding Available in Americas and AsiaInformation provided by Lubrizol |
|||
Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
RheTech Products CC40P100-01 40% Calcium Carbonate Reinforced Polypropylene, Black Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |