Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigm.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-GP1-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-GP1-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Low Flow Polycarbonate, 5% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-GP2-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Medium Flow Polycarbonate, 5% PTFE, General Purpose, Medium Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-GP3-TFE10 Polycarbonate, 10% PTFE, High Flow, Wear Resistant Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-GP3-TFE5 Polycarbonate, 5% PTFE, High Flow, Wear Resistant Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Middle Barrel Temperature | 299 - 338 °C | 570 - 640 °F | |
Polymer Resources PC-HH Polycarbonate, High Heat Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource.. |
|||
Middle Barrel Temperature | 299 - 338 °C | 570 - 640 °F | |
Polymer Resources PC-HH-UV Polycarbonate, High Heat, UV-stabilized Polycarbonate, High Heat, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Polymer Resources PC-GP1-TFE10 Polycarbonate, 10% PTFE, Wear Resistant, Low Flow Polycarbonate, 10% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
LTL Color Compounds ColorFast® PC60 Polycarbonate 6 melt extrusion gradeAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 299 - 321 °C | 570 - 610 °F | |
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 299 - 310 °C | 570 - 590 °F | |
A. Schulman ComAlloy Hiloy® 714 PPS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 299 - 310 °C | 570 - 590 °F | |
A. Schulman ComAlloy Hiloy® 754 Glass Reinforced, Flow Enhanced, PPS Alloy, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 299 - 310 °C | 570 - 590 °F | |
A. Schulman ComAlloy Hiloy® 758 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has b.. |
|||
Middle Barrel Temperature | 299 - 310 °C | 570 - 590 °F | |
A. Schulman ComAlloy Hiloy® 753 Glass Reinforced, Flow Enhanced, PPS Alloy, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 299 - 310 °C | 570 - 590 °F | |
A. Schulman ComAlloy Hiloy® 716 PPS, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 299 - 310 °C | 570 - 590 °F | |
A. Schulman ComAlloy Hiloy® 756 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |